High Temperature PP Fills/Infill for Round Type Cooling Tower
High temperature PP fills/infill for Round type cooling tower YN Round Type Cooling Tower Infill Feaures -This type of i
Basic Info
Model NO. | YN |
Noise Level | Low |
Application Fields | Industrial |
Certification | ISO, CTI |
Condition | New |
Transport Package | Woodencase 20gp/40gp Container |
Specification | 230/250/300/350 mm |
Trademark | NEWIN |
Origin | China |
HS Code | 8419909000 |
Production Capacity | 500000/Year |
Product Description
High temperature PP fills/infill for Round type cooling towerYN Round Type Cooling Tower Infill
Feaures -This type of infill made flame retardant PVC material, thermal formed by mold.
-The corrugated shape greatly increase the cooling area and greatly lengthen the time water keep on the surface of infill.
-The adoption of round type cooling tower infill makes round type cooling tower performance better and take smaller space.
Model--YN | PP |
Max.length | Depend on customer demand |
Width | 230/300/350 mm |
Continuous operation temperature | 85ºC |
Max. Application temp. (short term) | 90ºC |
Color | Green, black, blue, white (customizable) |
Corrugation height | 18 mm |
Installation method | Glued |
Trade Terms: EXW, FOB, CFR,CIF, DDU.
Payment term: T/T, L/C, West UnionMinimum Order Quantity: 1000pcs
YN Infill Pictures --- cooling tower cross flow film fill
Packing & Shipment
PVC Plastic sheet(after molding) Physical and mechanical property
No. | Item | symbol | unit | index | test method | |
1 | density | ρ | g/cm3 | ≤1.55 | GB/T 1033 1-2008 | |
2 | tensile strength | lengthways | σt | MPa | ≥42.0 | GB/T 13022-1991 |
crosswise | ≥38.0 | |||||
3 | tear strength | lengthways | σtr | kN/m | ≥150 | GB/T 1130-91 |
crosswise | ≥160 | |||||
4 | Folded in half Coldness Resistance Temperature | ordinary type | tb | ºC | ≤-8 | DL/T 742-2001 |
Frigostabile type | ≤-18 | |||||
5 | oxygen index | OI | -- | ≥30 | GB/T 2406 1-2008 |
GB/T 1033-1986 plastic density and relative density experiment method
GB/T 1040-1992 plastic tensile performance test methods
GB/T 1633-1979 thermoplastic softening point (d) test method
GB/T 1843-1996 plastic cantilever beam impact test method
GB/T 2406-1993 plastic combustion performance test method, oxidation index
GB/T 13022-1991 plastic film tensile performance test methods
GB/T 1190-1991 plastic rectangular tear performance test methods
Counter flow cooling tower infills